problem with new plaster

Discuss problem with new plaster in the Tiling Forum area at TilersForums.co.uk

paddy

Active Member
hi all
can anyone solve a problem for me I've recently tiled some new bathrooms only to discover 3 months later they've started to Dr bond off the walls
it was new plaster and I primed the walls with sbr and used powdered flexible adhesive so it's left me at a loss to what I've done wrong
any advice would be most welcome
 
OP
paddy

paddy

Active Member
2 weeks I'm kind of thinking it was wet plaster as it was in the middle of the really cold spell this winter
 
W

Waluigi

Unregistered (Please Register)
Was it a float and set or skim coat. Float and set needs much longer than two weeks.
 

Andy Allen

Metro specialist & forum entertainer!
Trusted Advisor
Professional Tiler
JOTM Winner
Should of been left for at least 6/7 weeks longer if no heating......or I would of used a dehumidifier...
 
OP
paddy

paddy

Active Member
it was 2 coat plaster and like I said earlier in the middle of the really cold spell so it looks like it was tiled too early
 